Grade Sb Sn Lead Copper Iron) Arsenic Zinc Aluminum Bismuth Other elements
  max %
1 4.0-5.0  90.0 – 92.0 0.35 4.0-5.0 0.08 0.10 0.005 0.005 0.08 0.10
2 7.0-8.0  88.0 – 90.0 0.35 3.0-4.0 .08 .10 .005 .005 .08 .10
3 7.5-8.5  83.0 – 85.0 0.35 7.5-8.5 .08 .10 .005 .005 .08 .10
4 12.0-14.0  80.5 – 82.5 0.25 5.0-6.0 .08 .10 .005 .005 - .10
5 9.5-10.5  61.0 – 63.0 24.0-26.0 2.5-3.5 .08 .15 .005 .005 - .30
6 14.0-16.0  4.5 – 5.5 79.0-81.0 0.50 .10 .20 .005 .005 - .50
7 14.0-16.0  9.3 – 10.7 74.0-76.0 0.50 .10 .60 .005 .005 - .50
10 14.5-17.5 0.75 – 1.25  78.0-83.0 0.60 .10 (3) .005 .005 -- .50
11 11.5-13.5  9.0 – 11.0  74.0-79.0 0.40-0.60 .10 .20 .005 .005 - .50
12 8.0-10.0  4.0 – 6.0 83.0-88.0 0.50 .10 .20 .005 .005 - .75

A narrower range of antimony within the limits stated may be specified, but the spread shall be not less than 1.00%; 0.80 to 1.40

Certificate of Analysis

Grade 2 Babbitt .078" Solid Wire

Laboratory Report: 7463
Tin B Balance
Lead .0750
Copper 3.4000
Arsenic < .0010
Bismuth .0060
Zinc .0010
Iron .0080
Silver .0170
Antimony 7.5900
Nickel .0020
Cadmium .0020
Aluminum < .0010
Gold .0010
Indium .0150

 

Grade 2 Babbitt .125" Solid Wire

Laboratory Report: 7536
Tin B Balance
Lead .0870
Copper 3.4000
Arsenic < .0010
Bismuth .0110
Zinc .0010
Iron .0030
Silver .0120
Antimony 7.63
Nickel .0020
Cadmium .0020
Aluminum .0010
Gold .0010